MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Sumitomo Bakelite Vyncolit® X684 Phenolic Novolac
Categories: Polymer; Thermoset; Phenolic; Phenolic, Novolac, Glass Filled

Material Notes: Vyncolit® X684 is a glass bead and glass fiber reinforced phenolic molding compound. It is a free ammonia grade with excellent mechanical properties.

Information provided by Sumitomo Bakelite High Performance Plastics (sbhpp)

Key Words: PF-(GB+GF)50
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.73 g/cc0.0625 lb/in³ISO 1183
Apparent Bulk Density 0.730 g/cc0.0264 lb/in³ISO 60
Water Absorption 0.16 %0.16 %ISO 62
Linear Mold Shrinkage 0.0031 cm/cm0.0031 in/inISO 2577
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 64.0 MPa9280 psiISO 527-1
Elongation at Break 0.93 %0.93 %ISO 527-1
Tensile Modulus 11.0 GPa1600 ksiISO 527-1
Flexural Strength 128 MPa18600 psiISO 178
Flexural Modulus 10.0 GPa1450 ksiISO 178
Flexural Strain at Break 1.53 %1.53 %ISO 178
Compressive Strength 205 MPa29700 psiISO 604
Charpy Impact Unnotched 0.900 J/cm²4.28 ft-lb/in²ISO 179-1
Charpy Impact, Notched 0.310 J/cm²1.48 ft-lb/in²ISO 179-1
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 200 °C392 °FISO 75 Af
Shrinkage 0.030 %0.030 %Post; ISO 2577
 
Descriptive Properties
ColorGreen

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Bakelite® PF 4136 Phenolic Molding Compound

PSUMIT505 / 194310

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.