MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Borealis Purpolen™ PP Y40-74 Polyethylene, post-consumer recycled
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Purpolen™ PP Y40-74 is a dark grey polypropylene (PP) post-consumer recycled supplied in pellets. This product is an ideal PP used where sustainability and circularity matter. It is a post-consumer recycled including a large part of recycled post-consumer waste coming from pre-sorted municipality waste. Purpolen™ PP Y40-74 is part of EuCertPlast certificate according to European Standard EN15343:2007 (certificate available upon request). Due to the nature of recycleds, some variation in color can be observed between batches.

Industry: Compounding & Masterbatch, Packaging, Home & Garden, Pipe, Fittings & Construction

Applications: Caps & Closures, Home & Garden, Rigid Industrial Packaging, Small Appliances, Under The Bonnet

Information provided by Borealis AG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.915 g/cc
Melt Flow 40.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PBORE9877 / 323234

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.