MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Chemical Concepts PERMATEX® #77 ULTRA BLUE® Multi-Purpose Gasket Maker
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: Permatex Ultra Blue RTV Silicone Gasket is a single component, room temperature vulcanizing gasketing compound designed to provide reliable “formed-in-place” gaskets for mechanical assemblies. This material cures on exposure to moisture in the air to form a tough, flexible, silicone rubber gasket. The product resists aging, weathering and thermal cycling without hardening, shrinking or cracking. Retains effective properties after contact with motor oil, transmission fluids, alcohol, and antifreeze solutions. Not recommended for parts in contact with gasoline. Not recommended for use in pure oxygen and / or oxygen rich systems.

Designed for superior bonding properties to oil contaminated metals as compared to other formed-in-place gaskets, and maintains outstanding oil resistance. NSF White Book registered.

Attributes: • Sensor safe, non-corrosive • Superior adhesion and flexibility • Improved oil resistance • Replaces most cut gaskets • Low odor • Can be used as a gasket maker or dressing • Non-flammable, Non-toxic. TYPICAL APPLICATIONS: • Pump housings • Machine tools • Compressors • Gearboxes • Transmission pans • Valve covers • Oil pans.

Information provided by Chemical Concepts™.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.30 g/ccuncured
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 30
@Temperature 25.0 °C
cured after 7 days @ 50% RH
Tensile Strength at Break 240 psicured after 7 days @ 50% RH
Elongation at Break 360 %cured after 7 days @25°C and 50% RH
 
Thermal PropertiesOriginal ValueComments
Flash Point >= 200 °Funcured
 
Processing PropertiesOriginal ValueComments
Extrusion Rate >= 880 g/min
@Temperature 25.0 °C
uncured
Cure Time 24.0 hourCures on exposure to air. Full cure in 24 hrs.
 
Descriptive Properties
ColorBlue non-sag paste, uncured
Gap Filling0.25 inches, cured after 7 days @25°C & 50% RH
Odorlow odor, uncured
Tack Free Time2 hrs tack free

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow SYL-OFF® 7367 CROSSLINKER
Chemical Concepts PERMATEX® ULTRA BLACK® Max Oil Resistance Gasket Maker
Momentive Performance Materials Silopren™ LSR 2050 Liquid Silicon Rubber - General Purpose
Parker Chomerics CHO-BOND® 116-19L Silicone Rubber Mixture

PCHEMI983 / 232198

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.