MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

A. Schulman NPP00GT02WH Minimal Mold Plate Out & Surface Bloom Unfilled, Flame-Retardant Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Flame Retardant

Material Notes: Minimal Mold Plate Out & Surface Bloom Unfilled, Flame-Retardant Polypropylene

Description:

Comments:
Testing and measurements were performed at 73 ± 3°F and 50± 5% relative humidity unless otherwise noted.
Hot Wire Ignition (HWI): 53 seconds as per UL 94 (Melt through with ignition).
California Furniture Testing: Passed as per TB 133.
Material Pre-dry: Normally it is not necessary to pre-dry this material. However, if conditions dictate drying to optimize material properties and part appearance then dry in a desiccant dryer at 180°F for 2-3 hours or 160°F for >4 hours.
Manifolds: Maintain manifolds, runners and tips 10 to 20°F above the front one temperature to allow easier filling. (Gate drool is best eliminated using screw decompression rather than reducing tip temperature.)
Back Pressure (Range): 50-100 psi. Injection Speed: medium to slow > depending on surface appearance. Screw Speed: medium. Injection Pressure: Adjust to just above a short shot. Injection Time: Adjust to just above a short shot. Cushion (Range): 0.2-0.5 in. Nozzle Type: Free flowing/Standard.
Some conditions may have to be altered to obtain acceptable parts. Please do not run too cold, molded in stress and rough surface may become a problem. If you must run below melt or temperatures recommended for dimensional precision you may compromise impact and esthetics. Retest parts to confirm performance.

Data provided by Ferro Corporation - Specialty Plastics Group.

A. Schulman has acquired the Ferro specialty plastics business.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.980 g/cc0.0354 lb/in³ASTM D792
Linear Mold Shrinkage 0.017 - 0.018 cm/cm0.017 - 0.018 in/inASTM D955
Melt Flow 11 g/10 min
@Load 2.16 kg,
Temperature 230 °C
11 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 29.0 MPa4200 psiASTM D638
Elongation at Break 50 %50 %ASTM D638
Flexural Yield Strength 36.5 MPa5300 psiASTM D790
Flexural Modulus 1.26 GPa183 ksiTangent; ASTM D790
Flexural Modulus, 1% Secant 1190 MPa172000 psiASTM D790
Izod Impact, Notched 0.694 J/cm1.30 ft-lb/inASTM D256
Izod Impact, Unnotched 13.3 J/cm25.0 ft-lb/inASTM D4812
Gardner Impact 27.1 J
@Temperature 23.0 °C
20.0 ft-lb
@Temperature 73.4 °F
M.F.E.; ASTM D5420
 
Electrical PropertiesMetricEnglishComments
Arc Resistance 127 sec127 secASTM D495
Comparative Tracking Index 580 V580 VASTM D3638
High Voltage Arc-Tracking Rate, HVTR 0.000 mm/min0.000 in/minASTM D495
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 65.0 °C149 °FUL 94 RTI
Deflection Temperature at 0.46 MPa (66 psi) 98.9 °C210 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 57.2 °C135 °FASTM D648
Flammability, UL94 V-2
@Thickness 3.17 mm
V-2
@Thickness 0.125 in
Listed
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 193 - 199 °C380 - 390 °F
Middle Barrel Temperature 199 - 204 °C390 - 400 °F
Front Barrel Temperature 204 - 210 °C400 - 410 °F
Nozzle Temperature 210 - 216 °C410 - 420 °F
Mold Temperature 21.1 - 32.2 °C70.0 - 90.0 °FCore. Cooler temperatures may be needed to maintain dimensions or eliminate sinks in thick sections.
 26.7 - 37.8 °C80.0 - 100 °FCavity
Drying Temperature 82.2 °C180 °F2-3 hrs at 180°F or 4+ hours at 160°F.
Dry Time 2 - 3 hour2 - 3 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PFERRO25 / 38139

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.