MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Solvay RHODAPEX® ES-2 Surfactant
Categories: Fluid

Material Notes: Description: Primary surfactant used in shampoos, bubble baths, shin cleansers and related cosmetic products.

Chemical Name: Sodium Laureth(2) Sulfate

CAS: 68585-34-2

Available in: Asia Pacific, Europe, Latin America and North America

Applications: RHODAPEX ES-2 is high foaming. For shampoos, bath products, skin cleansers and hand soaps.

Information provided by Rhodia, Rhodia has been acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
pH 6.5 - 7.56.5 - 7.510% Solution; RP-0402
Viscosity 2000 - 6000 cP2000 - 6000 cPRP-0596
 
Optical PropertiesMetricEnglishComments
Gardner Color Number <= 1.0<= 1.0RP-0138
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
Cloud point<5°CRP-0123
CompositionActive25-27%, EQ. WT. 382, RP-17501
 Free Oil<2%, RP-17303
 Sodium Chloride<1.5%, RP-0098
 Sodium Sulfate<1%, RP-0555

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay RHODAPEX® EA-2 Surfactant
Solvay RHODAPEX® EST-30/BLB Surfactant
Solvay RHODAPEX® ESC-70/AB Surfactant
Solvay RHODAPEX® ESB-70/A2 Surfactant
Solvay RHODAPEX® ESB-3/A2 Surfactant

WRHOD382 / 137613

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.