Dexflex thermoplastic polyolefins (TPOs) are in use in applications once reserved for more expensive engineering resins. The performance of these TPOs, combined with their quality and consistency, makes them cost-effective alternatives in automotive applications. Dexflex 1066LS-UV YGYA is a thermoplastic olefin elastomeric (TPO) typically used for automotive exterior applications that require excellent low-temperature toughness in large injection molded parts. Applications: Exterior Automotive Applications. Dexflex 1066LS-UV YZ9A BLACK is a thermoplastic olefin elastomeric (TPO) typically used for automotive exterior applications that require excellent low-temperature toughness in large injection molded parts. Information provided by LyondellBasell. |