MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Phillips 66 SynXPA® 100 R&O Oil
Categories: Fluid; Lubricant

Material Notes: Description: Conoco SynXPA R&O Oil lubricates stationary and portable rotary compressors, as well as reciprocating compressors that operate in severe service. It is useful in single- and double-acting, single- and multistage reciprocating compressors; in oil-flooded rotary-vane, rotary-lobe and screw compressors; in vacuum pumps that require an oil with low volatility; and in mild-duty industrial gear drives of spur, helical and bevel gear design that require an AGMA 3 or 4 R&O gear lubricant. It is not intended for use in applications which require extreme-pressure (EP) additives, such as spiral-bevel or hypoid gear sets. In ISO 32 and 68, it can be used in mild-duty hydraulic systems where the pump manufacturer specifies a rust- and oxidation-inhibited oil. SynXPA R&O Oil offers superior low-temperature fluidity and excellent high-temperature thermal and oxidative stability up to 400°F. It essentially eliminates the common problems of oil-separator varnishing and plugging, as well as vane sticking. With proper oil analysis, SynXPA R&O Oil can extend oil-drain intervals to 8,000 hours – compared to just 1,000 hours for conventional solvent-refined R&O oils. Do not use SynXPA R&O Oil for systems that require antiwear hydraulic oil. Do not mix it with conventional solvent-refined R&O oils or other synthetic oils.

Information provided by ConocoPhillips.

Phillips 66 Lubricants was spun-off from ConocoPhillips in 2012.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity Measurement 7373Viscosity Index
Saybolt Viscosity at 100°F 504 SUS504 SUS
Saybolt Viscosity at 210°F 58.2 SUS58.2 SUS
Kinematic Viscosity at 40°C (104°F) 95.9 cSt95.9 cSt
Kinematic Viscosity at 100°C (212°F) 9.7 cSt9.7 cSt
 
Thermal PropertiesMetricEnglishComments
Pour Point -34.4 °C-30.0 °F
Flash Point 250 °C482 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WCON189 / 75226

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.