MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
CHT AS1623 RTV, silicone adhesive sealant
Categories: Polymer; Thermoset; Silicone; Silicone, RTV, Adhesive/Sealant Grade

Material Notes: Description: This is a 1-part, RTV (Room Temperature Vulcanizing) silicone adhesive sealant. It is one in a range of Oxime cure products which are solvent free. It exhibits good primerless adhesion to many substrates especially plastics and cures rapidly at room temperature when in contact with atmospheric moisture. This product can be described as low corrosive but would not be recommended for use with copper or its associated alloys.

Key Features

  • High temperature resistance to +260°C/500°F
  • Resistance to 315°C/599°F intermittent exposure
  • Excellent flow and self leveling properties
  • Good adhesion to many substrates
Application: Applications include but are not limited to, sealing and fixing of domestic irons, shallow potting of electrical connectors for automotive applications.

Cured Product: 7 days at 23+/-2°C and 50+/-5% humidity

Information provided by CHT Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.08 g/ccBS ISO 2781
Brookfield Viscosity 9000 cPMixed
Storage Temperature <= 40.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 24ASTM D2240-95
Tensile Strength 131 psiISO 37
Elongation at Break 220 %ISO 37
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+13 ohm-cmASTM D-257
Dielectric Strength 409 V/milASTM D-149
 
Thermal PropertiesOriginal ValueComments
CTE, linear 300 µm/m-°C
Thermal Conductivity 0.200 W/m-K
Maximum Service Temperature, Air 250 °C
Minimum Service Temperature, Air -65.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 25.0 minTack Free Time / Skin Formation
 24.0 hour
@Temperature 23.0 °C
3mm Depth
Shelf Life 9.00 Month
 
Descriptive Properties
AppearanceViscous liquid
ColorRed
Cure typeOxime
RheologyFlowable
Self BondingYes
Volume Coefficient of Thermal Expansion902 ppm/°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCHTSIL019 / 314502

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.