MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Lubrizol Advanced Materials PEARLBOND® 522 Linear Thermoplastic Polyurethane
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Pearlbond™ 522 is a linear, polycaprolactone-copolyester polyurethane, supplied in form of white spherical granules with a very high crystallization rate and a very high thermoplasticity level.

Application: Pearlbond™ 522 can be added to formulations of REACTIVE POLYURETHANE HOT-MELTS (HMPUR), in order to improve the crystallisation speed.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.19 g/cc0.0430 lb/in³ISO 2781
Viscosity 4.90e+6 cP
@Temperature 130 °C
4.90e+6 cP
@Temperature 266 °F
Melt; ISO 1133
Melt Flow 105 - 160 g/10 min
@Load 2.16 kg,
Temperature 170 °C
105 - 160 g/10 min
@Load 4.76 lb,
Temperature 338 °F
ISO 1133
 
Chemical PropertiesMetricEnglishComments
Total Base Number <= 3.0<= 3.0mg KOH/g; MQSA 47 A
 
Thermal PropertiesMetricEnglishComments
Melting Point 65.0 - 69.0 °C149 - 156 °FMQSA 70 A
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.15 %<= 0.15 %MQSA 44
 
Descriptive Properties
Crystallization rate (minutes)9 - 11MQSA 12 B
ThermoplasticityVery highMQSA 68 A

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lubrizol Advanced Materials Pearlbond® 1160 Thermoplastic Polyurethane
Lubrizol Advanced Materials Pearlbond® 580 Thermoplastic Polyurethane
Lubrizol Advanced Materials PEARLBOND® 523 Linear Thermoplastic Polyurethane
Lubrizol Advanced Materials PEARLBOND® 521 Linear Thermoplastic Polyurethane
Lubrizol Advanced Materials PEARLBOND® 520 Linear Thermoplastic Polyurethane

PMES23 / 52921

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.