MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Schott GG455 Long Pass Filter
Categories: Ceramic; Glass; Optical; Filter

Material Notes: Colloidally colored glass. Data provided by the manufacturer, Schott Glas Mainz.

Similar glasses include GG395, GG400, GG420, GG435, GG385, GG475, GG495, OG515, OG530, OG550, OG570, OG590, RG610, RG630, RG645, RG665, RG695, RG715, RG780, RG830, RG850, RG1000, WG225, WG280, WG295, WG305, WG320

Key Words: DIN LP455
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.76 g/cc0.0997 lb/in³
 
Chemical PropertiesMetricEnglishComments
Acid Class, SR 4.44.4
Alkali Class, AR 11
Stain Resistance Class, FR 33
 
Thermal PropertiesMetricEnglishComments
CTE, linear  9.60 µm/m-°C
@Temperature -30.0 - 70.0 °C
5.33 µin/in-°F
@Temperature -22.0 - 158 °F
 10.6 µm/m-°C
@Temperature 20.0 - 300 °C
5.89 µin/in-°F
@Temperature 68.0 - 572 °F
Transformation Temperature, Tg 600 °C1110 °F
Glass Temperature Coefficient 0.0700.070
 
Optical PropertiesMetricEnglishComments
Refractive Index  1.53
@Wavelength 1014 nm
1.53
@Wavelength 1014 nm
Hg
 1.54
@Wavelength 587.6 nm
1.54
@Wavelength 587.6 nm
He
 1.55
@Wavelength 480 nm
1.55
@Wavelength 480 nm
Cd
Transmission, Visible  <= 0.0050 %
@Wavelength 400 - 440 nm
<= 0.0050 %
@Wavelength 400 - 440 nm
 88 - 90 %
@Wavelength 500 - 700 nm
88 - 90 %
@Wavelength 500 - 700 nm
Internal transmittance of 98-99% from 500-700 nm
IR Transmittance 91 %
@Wavelength 730 - 1600 nm
91 %
@Wavelength 730 - 1600 nm
Internal transmittance of 100%  from 730-1600 nm.
UV Transmittance 0.0010 %
@Wavelength 200 - 400 nm
0.0010 %
@Wavelength 200 - 400 nm
Internal transmittance of 0.001% or less from 200-400 nm.
Reflection Coefficient, Visible (0-1) 0.91
@Wavelength 587.6 nm
0.91
@Wavelength 587.6 nm
Reflection Factor P

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

CSGT27 / 2016

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.