MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Akro-Plastic Akromid® A3 ICF 30 black (5021) Nylon 66, 30% Carbon Fiber
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Carbon Fiber Filled

Material Notes: Carbon Fiber Reinforced Compounds. High strength. PA 6.6 CF 30.

Information provided by Akro-Plastic GmbH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.28 g/cc0.0462 lb/in³ISO 1183
Filler Content 30 %30 %ISO 1172
Linear Mold Shrinkage, Flow 0.0010 - 0.0030 cm/cm0.0010 - 0.0030 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm0.0050 - 0.0070 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 170 MPa24700 psi5 mm/min. Conditioned; ISO 527-2
 240 MPa34800 psi5 mm/min. Dry as Molded; ISO 527-2
Elongation at Break 1.8 %1.8 %5 mm/min. Dry as Molded; ISO 527-2
 3.5 %3.5 %5 mm/min. Conditioned; ISO 527-2
Tensile Modulus 15.0 GPa2180 ksi1 mm/min. Conditioned; ISO 527-2
 24.0 GPa3480 ksi1 mm/min. Dry as Molded.; ISO 527-2
Flexural Strength 265 MPa38400 psiConditioned. 2 mm/min; ISO 178
 370 MPa53700 psiDry as Molded. 2 mm/min; ISO 178
Flexural Modulus 14.0 GPa2030 ksi2 mm/min. Conditioned; ISO 178
 22.0 GPa3190 ksi2 mm/min. Dry as Molded; ISO 178
Charpy Impact Unnotched  5.50 J/cm²
@Temperature 23.0 °C
26.2 ft-lb/in²
@Temperature 73.4 °F
Dry as Molded; ISO 179-1/1eA
 5.50 J/cm²
@Temperature -30.0 °C
26.2 ft-lb/in²
@Temperature -22.0 °F
Dry as Molded; ISO 179-1/1eA
 7.00 J/cm²
@Temperature 23.0 °C
33.3 ft-lb/in²
@Temperature 73.4 °F
Conditioned; ISO 179-1/1eA
Charpy Impact, Notched  0.600 J/cm²
@Temperature -30.0 °C
2.86 ft-lb/in²
@Temperature -22.0 °F
Dry as Molded; ISO 179-1/1eA
 0.800 J/cm²
@Temperature 23.0 °C
3.81 ft-lb/in²
@Temperature 73.4 °F
Dry as Molded; ISO 179-1/1eA
 1.10 J/cm²
@Temperature 23.0 °C
5.23 ft-lb/in²
@Temperature 73.4 °F
Conditioned; ISO 179-1/1eA
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 10000 ohm10000 ohmConditioned; IEC 60093
 10000 ohm10000 ohmDry as Molded; IEC 60093
 
Thermal PropertiesMetricEnglishComments
Melting Point 262 °C504 °FDry as Molded. DES, 10°C/min; DIN EN 11357-1
Deflection Temperature at 1.8 MPa (264 psi) 254 °C489 °FDry as Molded; ISO 75
Flammability, UL94  HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
Conditioned
 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
Dry as Molded
 
Descriptive Properties
Burning Rate<100 mm/minDry as Molded. FMVSS 302. >1 mm thickness
 <100 mm/minConditioned. FMVSS 302. >1 mm thickness

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PAKRO9871 / 255528

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.