MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Okulen® 2000 PE-UHMW, SGB
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); UHMW PE (Ultra High Molecular Weight PE)

Material Notes: OKULEN® 2000 is an ultra high molecular low pressure polythylene with a molecular weight of > 7.000.000 g/mol plus additives for the improvement of specific material properties. It has an antistatic finish and additional lubricant for the conveyor industry. With added antioxidants, for example, which can be used at high temperatures. With additional flame retardant properties for use in rail vehicle, machinery and mining construction. With enhanced antibacterial effects.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.950 g/cc0.0343 lb/in³ISO 1183-A
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6565ISO 868
Tensile Strength, Yield >= 19.0 MPa>= 2760 psiISO/R 527
Elongation at Break >= 50 %>= 50 %ISO/R 527
Creep Strength 11.0 MPa1600 psi
Coefficient of Friction, Dynamic 0.080
@Pressure 2.00 MPa
0.080
@Pressure 290 psi
Metal=Rz 2.5, V = 150 mm/min; ASTM D1894
Coefficient of Friction, Static 0.13
@Pressure 2.00 MPa
0.13
@Pressure 290 psi
PE-metal, V = 10 m/min; ASTM D1894
Abrasion 6666Slurry-Test rel to GUR 4120 = 100%; DIN 58836
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 1.00e+14 ohm-cm<= 1.00e+14 ohm-cmTeil 30; IEC 600093 / VDE 0303
 
Thermal PropertiesMetricEnglishComments
CTE, linear 200 µm/m-°C111 µin/in-°FDIN 53752
Melting Point 135 - 137 °C275 - 279 °FISO 3146
Maximum Service Temperature, Air 80.0 °C176 °F
 
Compliance PropertiesMetricEnglishComments
FDA NoNo
 
Descriptive Properties
ColorLight grey

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Murtfeldt Original Material ”S”® plus + AB Polyethylene, Antibacterial
American Elements Z-MITE™ Zinc Oxide Nanopowder
Okulen® 2000 PE-UHMW, L
Okulen® 2000 PE-UHMW, DryRun
Okulen® 2000 PE-UHMW, 589 Blue

POKUL035 / 83477

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.