MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Avient OnFlex™ S HF 80A-3S1986 Thermoplastic Elastomer (TPE)
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: OnFlex™-S HF thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds utilize a unique, patent pending halogen free flame retardancy system. Furthermore, OnFlex™-S HF compounds offer good mechanical properties, compliance with UL94 V-0, good LOI values, wide hardness range, good processability, and excellent UV stability.

Properties are measured using injection molded plaques.

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.06 g/cc0.0383 lb/in³ISO 1183
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8080ISO 868
Tensile Strength at Break 5.50 MPa798 psiISO 37
Tensile Stress at Strain  3.00 MPa
@Strain 100 %
435 psi
@Strain 100 %
ISO 37
 4.20 MPa
@Strain 300 %
609 psi
@Strain 300 %
ISO 37
Elongation at Break 420 %420 %ISO 37
Tear Strength 35.0 kN/m200 pliISO 34-1
Compression Set  31 %
@Temperature 23.0 °C,
Time 259000 sec
31 %
@Temperature 73.4 °F,
Time 72.0 hour
ISO 815
 50 %
@Temperature 70.0 °C,
Time 79200 sec
50 %
@Temperature 158 °F,
Time 22.0 hour
ISO 815
 81 %
@Temperature 100 °C,
Time 79200 sec
81 %
@Temperature 212 °F,
Time 22.0 hour
ISO 815
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 550 V550 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
Flammability, UL94 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
UL 94
Oxygen Index 40 %40 %ISO 4589-2
Glow Wire Ignition Temperature 725 °C
@Thickness 2.00 mm
1340 °F
@Thickness 0.0787 in
IEC 60695-2-13
Glow Wire Flammability Index 960 °C
@Thickness 2.00 mm
1760 °F
@Thickness 0.0787 in
IEC 60695-2-12
 
Processing PropertiesMetricEnglishComments
Melt Temperature 160 - 180 °C320 - 356 °F
Mold Temperature 30.0 - 50.0 °C86.0 - 122 °F
Drying Temperature 80.0 °C176 °F
Dry Time 2.00 hour2.00 hour
 
Descriptive Properties
FeaturesFlame Retardant
FormsPellets
Generic MaterialTPE
Generic Material TypeStyrenic Thermoplastic Elastomer (TES)
Generic NameThermoplastic Elastomer (TPE)
Injection RateModerate-Fast
Processing MethodInjection Molding
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 South America
RoHS ComplianceRoHS Compliant
UsesAutomotive Applications
 Business Equipment
 Electrical/Electronic Applications
 General Purpose
 Industrial Applications

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Avient OnFlex™ S HF 90A-3S1988 Thermoplastic Elastomer (TPE)
AlphaGary Smokeguard™ O 208 Low Smoke Halogen Free
AlphaGary Smokeguard™ O 301 Low Smoke Halogen Free
AdvanSource Biomaterials ChronoFlex® AL 80A Biodurable Medical Grade Polyurethane
Avient OnFlex™ S EH 80A-3S7005 Thermoplastic Elastomer (TPE)

PH0POL1163 / 145732

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.