MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Cabot MONARCH® 120 Specialty Carbon Black
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Product highlights: MONARCH 120 specialty carbon black is a general purpose low color pigment black suitable for a broad range of tinting applications. Easy to disperse, this economical pigment black can enable higher loadings in most systems.

Key applications: MONARCH 120 specialty carbon black offers very blue undertone and high loading opportunities. It is a cost effective opacifying agent and offers excellent rub resistance as well as good viscosity and flow properties.
Printing inks: MONARCH 120 specialty carbon black is suitable for use in web offset, coldset and letter press printing inks.
General industrial coatings: MONARCH 120 specialty carbon black is also suitable for use in general industrial coatings where high jetness is not required.
Tinting applications: MONARCH 120 specialty carbon black is suitable for use in tinting applications. The dispersability of MONARCH 120 specialty carbon black depends on the equipment used and the formulation. Like most low color pigment blacks, it exhibits ease of dispersion characteristics because of its relatively large particle size.

Information provided by Cabot Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Particle Mesh Size 325 Mesh<200 ppm residue; ASTM D-1514
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 1.0 %ASTM D-1509
 
Descriptive Properties
Iodine absorption30 mg/gCTM 23.4, Devolatilized
OAN70 cc/100gASTM D-2414
Product Formfluffy
Tint0.58ASTM D-3265

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCABOT159 / 315894

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.