MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Polycasa SPC UK Polycarbonate Multiwall Sheet
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: QUINN SPC UK has variety of characteristics and benefits including
  • High impact resistance
  • Weather resistant
  • High heat and sound insulation
  • Long life span
  • Excellent light transmission
  • Transparent
  • Resistant to chemicals
  • Light Weight
  • Superb thermal insulation

  • Roofing and glazing
  • Swimming pool enclosures
  • Cladding
  • Conservatories
  • Skylights
  • Boxes
  • Shelters
  • Protective covers for fragile items
  • Vaults
  • Advertising panels
  • Suspended ceilings
  • Winter gardens
  • Partitions Pergolas

Quinn Manufacturing Group rebranded its Plastics Division as Polycasa in 2013.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Apparent Bulk Density 0.140 g/cc25 mm - 5 wall
 0.170 g/cc10 mm - 2 wall
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.0290 W/m-K10 mm - 2 wall
 0.0425 W/m-K25 mm - 5 wall
Maximum Service Temperature, Air 130 °C
Minimum Service Temperature, Air -40.0 °C
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 14 %Opal, 25mm - 5 wall
 17 %Bronze Opal, 25mm - 5 wall
 17 %Bronze, 25mm - 5 wall
 37 %Bronze, 10mm - 2 wall
 45 %Opal, 10mm - 2 wall
 62 %Clear, 25mm - 5 wall
 88 %Clear, 10mm - 2 wall
UV Transmittance 34 %Opal, 25mm - 5 wall
 39 %Bronze, 25mm - 5 wall
 40 %Bronze Opal, 25mm - 5 wall
 63 %Clear, 25mm - 5 wall

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI E 52100 Steel (100Cr6, SUJ2, UNS G52986)
Armacell Ensolite™ FC0 (Fine Cell) Continuous Rolls/Sheets, PVC/NBR
Alliance N-40SH Neodymium Iron Boron Magnetic Material
Tungsten, W
SunChemical Gwent P2121112P9 Tetrafluoromethane Plasma Modified Multiwalled Carbon Nanotubes

PSF023D / 66594

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.