MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Avient PolyAdd™ 2928 Purge PEC Purge Compound  (discontinued **)
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer; Thermoplastic; Purging Compound

Material Notes:

2928 Purge PEC is a compound designed to facilitate color changes and other formulation changes by purging out the flow channels with less material. It is particularly beneficial in extrusion operations that do not run 24 hours a day 7 days per week. By cooling the extruder down and running 2928 through to the die so that all channels are full when the extruder is shut down for a day or two, start up is facilitated by the purge compound.

Description/Features:

  • Purging Compound

Market:

  • Film

Processing Method:

  • Blown Film
  • Cast Film

Note: The additive package contained in 2928 Purge PEC is designed to help gently removing deposits that have built up during operation as well as preventing further degradation. This combination of ingredients is formulated to polish the metal surface free of color and charred material without being excessively abrasive. Acceptable for FDA applications depending on end use.

Information provided by PolyOne Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Descriptive Properties
AdditiveProprietary Blend
Base ResinPolyethylene
Product FormUnderwater Cut Pellets

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
OJSC Plastic ABS 20F ABS Impact and Heat Modifier
Lushan PA6+30% GF Nylon Toughener/PA Impact Modifier
Emerald Performance Materials ERISYS™ GE-6 Epoxy Functional Reactive Modifier
Emerald Performance Materials ERISYS™ GE-5 Epoxy Functional Reactive Modifier
Dow SYL-OFF® PMCP7615 Release Modifier

PH1PO3062 / 44871

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.