This Valite product has been replaced by Plenco 4246. Data provided by Plenco. VALITE 1246-18X is a black two-stage, medium heat resistant phenolic molding compound. It has excellent electrical, moldability and molded finish characteristics. It is used in applicance applications and can be molded by compression, transfer, or injection. Plenco drop ball 113g test value is 27 cm. Plenco has discontinued their Valite product line. |