MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Refractory Metals

Plansee Molybdenum Sputtering Target
Categories: Metal; Nonferrous Metal; Molybdenum Alloy; Pure Element

Material Notes: High purity, maximum density, and homogeneous microstructure. Molybdenum coatings are the crucial components of the thin-film transistors used in TFT-LCD screens. These provide instantaneous control of the individual image dots (pixels) and consequently ensure particularly sharp image quality. Molybdenum layers are also used as back contacts in CIGS solar cells.

Targets are used in the magnetron sputtering method, whereby tiny metal particles are vaporized from the sputtering targets and are then deposited as a thin film.

Information provided by PLANSEE.

Vendors: PLANSEE SE: Whether it's high temperatures, aggressive chemicals or extreme mechanical loading: PLANSEE supplies a suitable product solution in refractory metals or composite materials. As the world market leader in powder metallurgically produced high performance materials we combine outstanding materials knowledge with profound applications and technology know-how. Visit us at www.plansee.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density >= 10.2 g/cc>= 0.368 lb/in³
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000560 ohm-cm
@Temperature 20.0 °C
0.00000560 ohm-cm
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear 5.20 µm/m-°C
@Temperature 20.0 °C
2.89 µin/in-°F
@Temperature 68.0 °F
Thermal Conductivity 140 W/m-K
@Temperature 20.0 °C
972 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 0.0010 %0.0010 %<10 ppm by weight
Arsenic, As 0.00050 %0.00050 %<5 ppm by weight
Cadmium, Cd 0.00050 %0.00050 %<5 ppm by weight
Calcium, Ca 0.0020 %0.0020 %<20 ppm by weight
Carbon, C 0.0030 %0.0030 %<30 ppm by weight
Chromium, Cr 0.0020 %0.0020 %<20 ppm by weight
Cobalt, Co 0.0010 %0.0010 %<10 ppm by weight
Copper, Cu 0.0020 %0.0020 %<20 ppm by weight
Hydrogen, H 0.0010 %0.0010 %<10 ppm by weight
Iron, Fe 0.0020 %0.0020 %<20 ppm by weight
Lead, Pb 0.00050 %0.00050 %<5 ppm by weight
Magnesium, Mg 0.0010 %0.0010 %<10 ppm by weight
Manganese, Mn 0.00020 %0.00020 %<2 ppm by weight
Mercury, Hg 0.00010 %0.00010 %<1 ppm by weight
Molybdenum, Mo >= 99.97 %>= 99.97 %
Nickel, Ni 0.0010 %0.0010 %<10 ppm by weight
Nitrogen, N 0.0010 %0.0010 %<10 ppm by weight
Oxygen, O 0.0040 %0.0040 %<40 ppm by weight
Potassium, K 0.0020 %0.0020 %<20 ppm by weight
Silicon, Si 0.0020 %0.0020 %<20 ppm by weight
Silver, Ag 0.0010 %0.0010 %<10 ppm by weight
Sodium, Na 0.0010 %0.0010 %<10 ppm by weight
Tin, Sn 0.00050 %0.00050 %<5 ppm by weight
Titanium, Ti 0.0010 %0.0010 %<10 ppm by weight
Tungsten, W 0.030 %0.030 %<300 ppm by weight
Vanadium, V 0.0010 %0.0010 %<10 ppm by weight
Zinc, Zn 0.0010 %0.0010 %<10 ppm by weight
 
Descriptive Properties
Purity>99,97%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

NPLAM970 / 249324

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.