Product Description: LD 156 series are LDPE grades, specially designed for lamination films and co-extruded films. They offer good mechanical, stiffness and optical properties, combined with very low gel level. These grades have a Film Appearance specification. Two additive packages are available tailored to the needs of the laminator. LD 156 is manufactured with narrow specifications to suit the high consistency requirements of lamination films. Availability: Africa & Middle East and Europe Additive: - Antiblock: 1500 ppm
- Slip: 550 ppm
- Thermal Stabilizer: Yes
Applications: - Blend Partner
- Co-Extrusion Films
- Collation Shrink
- Form Fill and Seal Packaging
- Freezer Film
- Higher Quality Lamination
- Lamination Film
- Medium Duty Shrink Film
- Shoppers
Information provided by ExxonMobil |