MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Overview of materials for Linear Low Density Polyethylene (LLDPE), Rotational Molding Grade
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Rotational Molding Grade

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Rotational Molding Grade". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.913 - 0.945 g/cc0.0330 - 0.0341 lb/in³Average value: 0.935 g/cc Grade Count:75
Environmental Stress Crack Resistance 24.0 - 1000 hour24.0 - 1000 hourAverage value: 565 hour Grade Count:39
 38.0 - 400 hour
@Temperature 50.0 - 50.0 °C
38.0 - 400 hour
@Temperature 122 - 122 °F
Average value: 450 hour Grade Count:9
 28.0 - 400 hour
@Temperature 50.0 - 50.0 °C
28.0 - 400 hour
@Temperature 122 - 122 °F
Average value: 450 hour Grade Count:5
 28.0 - 400 hour
@Thickness 2.00 - 2.00 mm
28.0 - 400 hour
@Thickness 0.0787 - 0.0787 in
Average value: 450 hour Grade Count:5
Melt Flow 1.00 - 10.4 g/10 min1.00 - 10.4 g/10 minAverage value: 4.97 g/10 min Grade Count:75
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 52.0 - 61.052.0 - 61.0Average value: 57.6 Grade Count:11
Tensile Strength, Ultimate 17.0 - 30.1 MPa2470 - 4370 psiAverage value: 24.2 MPa Grade Count:16
Tensile Strength, Yield 10.0 - 22.8 MPa1450 - 3300 psiAverage value: 17.9 MPa Grade Count:68
Elongation at Break 239 - 1100 %239 - 1100 %Average value: 731 % Grade Count:32
Elongation at Yield 10.0 - 20.6 %10.0 - 20.6 %Average value: 15.1 % Grade Count:41
Modulus of Elasticity 0.260 - 0.700 GPa37.7 - 102 ksiAverage value: 0.519 GPa Grade Count:4
Flexural Modulus 0.245 - 1.05 GPa35.5 - 152 ksiAverage value: 0.677 GPa Grade Count:65
Charpy Impact, Notched 0.730 - 8.70 J/cm²3.47 - 41.4 ft-lb/in²Average value: 3.44 J/cm² Grade Count:3
Tensile Impact Strength 104 - 104 kJ/m²
@Temperature -30.0 - -30.0 °C
49.5 - 49.5 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 104 kJ/m² Grade Count:1
Dynatup @ -30°C 61.0 - 81.3 J45.0 - 60.0 ft-lbAverage value: 71.2 J Grade Count:6
 
Thermal PropertiesMetricEnglishComments
Melting Point 104 - 128 °C220 - 262 °FAverage value: 125 °C Grade Count:50
Crystallization Temperature 105 - 113 °C221 - 235 °FAverage value: 111 °C Grade Count:16
Deflection Temperature at 0.46 MPa (66 psi) 49.0 - 70.0 °C120 - 158 °FAverage value: 56.9 °C Grade Count:46
Deflection Temperature at 1.8 MPa (264 psi) 37.0 - 42.0 °C98.6 - 108 °FAverage value: 38.7 °C Grade Count:28
Vicat Softening Point 91.0 - 118 °C196 - 244 °FAverage value: 111 °C Grade Count:20
Heat Distortion Temperature 41.0 - 60.0 °C106 - 140 °FAverage value: 50.6 °C Grade Count:9
Brittleness Temperature -70.0 - -60.0 °C-94.0 - -76.0 °FAverage value: -66.2 °C Grade Count:13
Flammability, UL94 V-2V-2Grade Count:3
Oxygen Index 26.0 %26.0 %Average value: 26.0 % Grade Count:3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Bamberger Polymers Bapolene® 3042U Polyethylene, Rotational Molding Grade
Overview of materials for Medium Density Polyethylene (MDPE), Rotational Molded
Overview of materials for High Density Polyethylene (HDPE), Rotational Molding Grade
Overview of materials for Linear Medium Density Polyethylene (LMDPE), Rotational Molded
Overview of materials for Linear Low Density Polyethylene (LLDPE), Injection Molded

O3855 / 78261

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.