MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Parson Adhesives PARLITE® 4725 UV Glue and UV Adhesive for Electronic Assembly
Categories: Polymer; Adhesive

Material Notes: Application: Specifically designed for potting. Bonds with slight adhesion: for connectors, thermal switches, temper proofing.

Information provided by Parson Adhesives, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity 600 - 800 cP600 - 800 cP
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5555
Tensile Strength 5.17 MPa750 psi
Elongation at Break 72 %72 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Parson Adhesives PARLITE® 4760 UV Glue and UV Adhesive for Electronic Assembly
Envalior Stanyl® TW200F6 PA46-GF30, Dry, 30% Glass Filled, Heat Stabilized
Envalior Stanyl® TE250F6 PA46-GF30 FR(17), Dry, 30% Glass Filled, Heat Stabilized, Flame Retardant
Parson Adhesives PARLITE® 4710 UV Glue and UV Adhesive for Electronic Assembly
Parson Adhesives PARLITE® 4750 UV Glue and UV Adhesive for Electronic Assembly

PPARSN083 / 186526

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.