MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Phillips 66 Tacna® HD Grease NLGI Grade 2
Categories: Fluid; Lubricant; Lithium Gellant; Organic Soap Gellant

Material Notes: Tacna HD is a premium quality, adhesive, extreme-pressure (EP) lithium complex grease developed for the lubrication of heavily loaded construction, mining and industrial equipment. It also is recommended for use as a chassis grease for heavy mobile equipment. It is formulated to provide long service life in severe service applications. Tacna HD is manufactured with high-quality, high-viscosity base oils and a lithium complex soap thickener. It is fortified with extreme-pressure and antiwear additives, rust and oxidation inhibitors, and a tackiness additive. It has excellent oxidation resistance, high load-carrying capacity for excellent wear protection, and protects metal parts against rust and corrosion. It has excellent adhesion to bearing surfaces for improved retention and resistance to water washout, and has excellent resistance to structural breakdown even under severe operating conditions.

Applications:

  • Heavily loaded plain and rolling-element bearings in industrial and off-road equipment
  • Chassis parts on heavy mobile equipment
  • Construction equipment
  • Dredging equipment
  • Marine deck equipment
  • Offshore drilling equipment
  • Rock quarry equipment
Features/Benefits:
  • High load-carrying capacity
  • Excellent shock-load resistance
  • Excellent oxidation resistance
  • Adhesive to metal surfaces
  • High shear stability
  • Protects against rust and corrosion
  • Excellent resistance to water washout

Phillips 66 Lubricants was spun-off from ConocoPhillips in 2012.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.15 lb/gal
Viscosity Measurement 87Viscosity Index (Base Oil Property)
Saybolt Viscosity at 100°F 2150 SUSBase Oil Property
Saybolt Viscosity at 210°F 129 SUSBase Oil Property
Kinematic Viscosity at 40°C (104°F) 400 cStBase Oil
Kinematic Viscosity at 100°C (212°F) 26 cStBase Oil
Oxidative Stability 100 hour
@Pressure 0.304 MPa
Pressure Drop; ASTM D942
 
Mechanical PropertiesOriginal ValueComments
Four Ball Extreme Pressure, Weld Load 315 kgASTM D2596
Four Ball Wear 0.450 mmScar Wear; ASTM D2266
Penetration P(60), 1/10 mm 265 - 295ASTM D217
Timken Test 55.0 lbASTM D2509
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 177 °C
Minimum Service Temperature, Air -12.0 °C
Dropping Point >= 500 °F
 
Descriptive Properties
ColorRed
Copper Corrosion1bASTM D4048
Rust Test A&BPass
Soap Type (Thickener)Lithium Complex
TextureSmooth/Tacky
Water Washout2%ASTM D-1264, @ 175°F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WCON233 / 75270

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.