Product highlights: CABELEC CA6741 is an electrically conductive compound based on carbon black and a polyacetal copolymer. Its electrical properties are permanent and are not dependent on atmospheric conditions. The compound can easily be processed on conventional molding equipment. Key applications: CABELEC CA6741 conductive compound is principally recommended for applications where freedom from the hazard of electrostatic discharge is necessary. Examples of use are in handling of explosive powders, pigments, liquids and electronic components. Information provided by Cabot Corporation |