MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Mitsubishi Reny® 1507 Polyamide
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes: 30% glass fiber mineral reinforced non-halogen. Flame retardant grade. High Performance Polyamide. Reny is a proprietary molding compound based on mainly polyamide MXD6 that has been reinforced with glass fiber, carbon fiber or special minerals. Reny generally has superior mechanical strength and modulus compared with other engineering plastics. Thus, Reny is suitable as a metal substitute in many applications, including automobiles, electronics, electrical appliances, machinery, and construction. Excellent mechanical strength and modulus over a wide range of temperatures. Superior to commodity polyamides in dimensional stability and mechanical strength due to low water absorption. Low thermal expansion coefficient, equivalent to that of metal alloys. Highly resistant to oils and organic solvents. Low mold shrinkage and low warpage. Good surface finish even in highly filled grades.

Information provided by Mitsubishi Engineering Plastics Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.51 g/ccISO 1183
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 169 MPadry; ISO 527-1,2
Elongation at Break 1.8 %dry; ISO 527-1,2
Tensile Modulus 12500 MPadry; ISO 527-1,2
Flexural Strength 288 MPadry; ISO 178
Flexural Modulus 12000 MPadry; ISO 178
Charpy Impact Unnotched 52.0 kJ/m²dry; ISO 179-1, 179-2
Charpy Impact, Notched 7.80 kJ/m²dry; ISO 179-1, 179-2
 
Electrical PropertiesOriginal ValueComments
Comparative Tracking Index 325 Vdry; IEC 60112
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 222 °Cdry; ISO 75-1,2
Flammability, UL94 V-0
@Thickness 1.60 mm
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 270 °C
Middle Barrel Temperature 265 °C
Front Barrel Temperature 260 °C
Nozzle Temperature 270 °C
Mold Temperature 120 - 145 °C
Injection Pressure 20.0 - 150 MPa
Screw Speed 60 - 150 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mitsubishi Reny® 1025 Polyamide
Mitsubishi Reny® 1035 Polyamide
Mitsubishi Reny® 1527 Polyamide
Mitsubishi Reny® 1021UCS Polyamide
Mitsubishi Reny® 1022HS Polyamide

PMITSU9027 / 191700

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.