MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

AM-350 Stainless Steel Plate, Sheet, Strip, Condition H850, UNS S35000
Categories: Metal; Ferrous Metal; Stainless Steel; T S30000 Series Stainless Steel

Material Notes:

Information provided by ATI and the references(s).

Key Words: ASTM A 693
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.81 g/cc0.282 lb/inĀ³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell C >= 42>= 42
Tensile Strength 1275 MPa184900 psi
Tensile Strength, Yield 1030 MPa149000 psi
 
Component Elements PropertiesMetricEnglishComments
Chromium, Cr 16.5 %16.5 %
Iron, Fe 76 %76 %as balance
Manganese, Mn 0.80 %0.80 %
Molybdenum, Mo 2.75 %2.75 %
Nickel, Ni 4.3 %4.3 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AM-350 Stainless Steel, Annealed Plate, Sheet, Strip, UNS S35000
AISI 3150 Steel (UNS G31500)
AISI Type S24000 Stainless Steel, plate
3RE60 Duplex Stainless Steel, Annealed Tube, UNS S31500
AM-350 Stainless Steel Plate, Sheet, Strip, Condition H1000, UNS S35000

MQZ9929 / 172179

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.