MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
IBC Advanced Alloys C17510 Beryllium Copper Alloy Plate, Temper AT(TF00)
Categories: Metal; Nonferrous Metal; Beryllium Alloy; Copper Alloy

Material Notes: C17510 - Beryllium Copper mold alloys have hardnesses comparable to tool steel, but with superior thermal conductivity. Beryllium copper plate, block, bar and rounds -- upset forged and heat treated to multiple tempers -- are available in a choice of strength, hardness and thermal conductivity levels.

C17510 Beryllium Copper is manufactured to provide a good strength with even better thermal conductivity than C17200. This copper alloy offers conductivity of 45 to 60 percent of pure copper while providing significant strength and hardness properties. This copper alloy is often used in the resistance welding industry.

Information provided by IBC Advanced Alloys.

Key Words: UNS C17510
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.319 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell B 92 - 100
Tensile Strength 100000 - 130000 psi
Tensile Strength, Yield 80000 - 100000 psi
@Strain 0.2 %
Elongation at Break >= 10 %
Modulus of Elasticity 20000 ksi
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity <= 0.00000380 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 9.80 µin/in-°F
Thermal Conductivity 1680 BTU-in/hr-ft²-°F
Melting Point 1900 - 1980 °F
Solidus 1900 °F
Liquidus 1980 °F
 
Component Elements PropertiesOriginal ValueComments
Beryllium, Be 0.20 - 0.60 %
Copper, Cu 97.2 - 98.4 %As Balance
Nickel, Ni 1.4 - 2.2 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Beryllium Copper, UNS C17200, TH04 Temper rod, bar, plate, tubing, >25 mm
IBC Advanced Alloys C17510 Beryllium Copper Alloy Plate, Temper A(TB00)
Bohler-Uddeholm BeCu Alloy 172 Mold Material
Cadi MOLD-MOR™ 3
IBC Advanced Alloys C17510 Beryllium Copper Alloy Rounds, Temper A(TB00)

NIBCA175B / 177687

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.