MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Aurora Plastics TufFlex™ GA-509-75 TPE Compound
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Application: A UL listed, sunlight resistant, 75°C rated, UL1277 power limited and control cable jacketing compound for CMX, CL2 and CL3 applications.

Information provided by S&E Specialty Polymers; S&E Specialty Polymers was aquired by Aurora Plastics in 2017.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.40 g/cc1.40 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 75
@Time 15.0 sec
75
@Time 0.00417 hour
ASTM D2240
Tensile Strength 11.8 MPa1710 psiASTM D412
 11.8 MPa
@Temperature 100 °C,
Time 864000 sec
1710 psi
@Temperature 212 °F,
Time 240 hour
Aged
Elongation at Break 385 %385 %ASTM D412
 327.25 %
@Treatment Temp. 100 °C,
Time 864000 sec
327.25 %
@Treatment Temp. 212 °F,
Time 240 hour
Aged
100% Modulus 7.93 MPa
@Strain 100 %
1150 psi
@Strain 100 %
ASTM D412
 
Thermal PropertiesMetricEnglishComments
Oxygen Index 28 %28 %ASTM D2863
 
Processing PropertiesMetricEnglishComments
Processing Temperature 171 - 182 °C340 - 360 °FSuggested Stock

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
SCG Chemicals EL-Pro™ P722JO Polypropylene Injection Molding

PSEPN018 / 179022

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.