MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Westlake LF2040 Hexene Linear Low Density Polyethylene  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE)

Material Notes: Westlake LF2040 is a hexene LLDPE with excellent physical properties and heat sealing characteristics, which allow for down-gauging and blending with other materials. Typical applications include stretch films, heavy duty bags and sacks, agricultural films, and trash bags & liners. This Kosher compliant material is available with various slip and antiblock levels.

    Application/Uses
  • Bags and sacks
  • Agricultural films
  • Trash bags and liners
  • Co-extruded structures

FDA: This material complies with FDA regulations in 21 CFR, section 177.1520. Kosher Compliant.

All information provided by Westlake Chemical

Key Words: Excellent physical properties and heat sealing characteristics
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.918 g/ccASTM D1505
Thickness 1.00 mil
Melt Flow 2.0 g/10 minASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 9.65 MPa
Film Tensile Strength at Yield, TD 9.65 MPa
Film Elongation at Break, MD 500 %ASTM D882
Film Elongation at Break, TD 900 %ASTM D882
Elmendorf Tear Strength, MD 200 g/mil
Elmendorf Tear Strength, TD 650 g/mil
Dart Drop 90.0 g/milASTM D1709
Film Tensile Strength at Break, MD 8000 psiASTM D882
Film Tensile Strength at Break, TD 4800 psiASTM D882
1% Secant Modulus, MD 20000 psiASTM D882
1% Secant Modulus, TD 22000 psiASTM D882
 
Optical PropertiesOriginal ValueComments
Haze 2.5 %ASTM D1003
Gloss 95 %45°
 
Processing PropertiesOriginal ValueComments
Melt Temperature 400 - 420 °F
Blow-up Ratio (BUR) 2.5
 
Descriptive Properties
ProcessFilm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Westlake LF2050 Hexene Linear Low Density Polyethylene
Refractory 26 Nickel Alloy Composition Spec
Ozhennite 0.5 Zirconium Alloy, Composition Spec
Overview of materials for AISI 1000 Series Steel
Excel Zirconium Alloy, Composition Spec

PWESF8927 / 133278

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.