MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Chemical Concepts Chem-Set™ RTV 6500 Acetoxy cure silicone sealant and adhesive
Categories: Polymer; Adhesive; Thermoset; Silicone; Silicone, RTV, Adhesive/Sealant Grade

Material Notes: Chem-set™ RTV 6500 Silicone is a Heat Resistant Sealant is a one-part, nonslumping paste that cures to a rubbery solid at room temperature on exposure to water vapor in the air. This silicone product is formulated to perform at temperatures ranging from -65 to 260º (-85 to 500ºF) for continuous operation and to 315ºC (600ºF) for intermittent exposure. It can be used for numerous sealing and bonding applications. APPLICATIONS: The high temperature properties of this sealant make it ideally suited for: Sealing and encapsulating heating elements in appliances, Aerospace gasketing, Moving oven belts, Industrial ovens, Bag filters on smoke stacks, Other critical bonding, sealing, potting, encapsulating and protective coatings, where parts must perform at high temperatures.

Information provided by Chemical Concepts™.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.04 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 26
@Temperature 25.0 °C
cured after 72 hrs & 50% RH
Tensile Strength 350 psicured 72 hrs, @ 25°C, & 50% RH
Elongation at Break 600 %Cured 72 hrs @ 25°C, & 50% RH
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 500 °Fcontinuous
 600 °Fintermittent
Minimum Service Temperature, Air -85.0 °Fcontinuous
 
Processing PropertiesOriginal ValueComments
Extrusion Rate >= 90.0 g/min1/8 inch orifice, @ 90 psi
Cure Time 24.0 hour
@Temperature 25.0 °C
1/8 inch thickness, 50% RH
 
Descriptive Properties
Colorred
Tack Free Time17 minutes, exposed to air, 25°C, and 50% RH

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aremco Aremco-Seal™ 4030 High Temperature Specialty Coatings Silicone, Ceramic Filled
Aremco Aremco-Bond™ 598 Conductive Epoxy Adhesive
Aremco Aremco-Bond™ 2335 Ultra High Temperature Epoxy
Dow 3-4680 SILICONE GEL KIT
Dow 3120 RTV SILICONE RUBBER

PCHEMI951 / 232213

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.