MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
3M Scotch-Weld™ TE100 Black Polyurethane Reactive Adhesive
Categories: Polymer; Adhesive; Thermoset; Polyurethane, TS

Material Notes: 3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as wood, fiber reinforced plastic (FRP) and many other plastics to themselves, to metal and glass. Extrudable grade adhesive with medium set time and low viscosity ideal for bonding wood. Bonds selected plastics. Yields thin glue lines.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density >= 1.05 g/cc
Brookfield Viscosity 9000 cPThermosel using spindle #27
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 57
Tensile Strength at Break 26.5 MPaASTM D638 Die C
Elongation at Break 675 %ASTM D638 Die C
Tensile Modulus 7500 psiASMT D638 Die C
Shear Strength 550 psi
@Temperature 82.0 °C
Overlap, Maple
 710 psi
@Temperature 23.0 °C
Overlap, Polystyrene, Substrate Failure
 990 psi
@Temperature 23.0 °C
Overlap, ABS
 1150 psi
@Temperature 82.0 °C
Overlap, FRP
 1330 psi
@Temperature 23.0 °C
Overlap, Polyacrylic, Substrate Failure
 1720 psi
@Temperature 23.0 °C
Overlap, Polycarbonate
 1900 psi
@Temperature 23.0 °C
Overlap, PVC, Substrate Failure
 2100 psi
@Temperature 23.0 °C
Overlap, Maple
 3160 psi
@Temperature 23.0 °C
Overlap, FRP
Peel Strength 1.00 pli180°, Aluminum
 1.00 pli180°, Glass
 11.0 pli180°, Polystyrene
 65.0 pli180°, ABS, Cotton duck failed during testing
 78.0 pli180°, PVC, Cotton duck failed during testing
 80.0 pli180°, FRP, Cotton duck failed during testing
 80.0 pli180°, Polyacrylic, Cotton duck failed during testing
 101 pli180°, Polycarbonate, Cotton duck failed during testing
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 121 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 1.00 minSet Time
 
Descriptive Properties
AppearanceBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Epoxy Adhesive, Flexible
Abatron AboCast/AboCure 8110-2 Flexible Epoxy
Abatron AboCast 8110-7/AboCure 8110-1 Flexible Epoxy
Abatron AboCast 8110-6/AboCure 8110-1 Flexible Epoxy
Abatron AboCast 8110-2/AboCure 8110-1 Flexible Epoxy

PMM34766 / 169513

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.