The Trithene® TX 7010 resin is a low-density polyethylene (LDPE) with high molecular weight, excellent processability with very good mechanical properties. Besides these properties, the material is characterized by excellent draw-down and shrinkage properties. Contains no additives. This product complies with ASTM standard D1248-IA4 and the requirements of Brazilian and corresponding legislation of Mercosul and it is in conformity with FDA Regulations 21 CFR 177.1520 (c) 2.1, to contact with foodstuff. Applications: Thin and general purpose films. Thin shrink film. Coextrusion with PA (Nylon), EVA, PP. Resin Properties: Compressed molded plate. Method ASTM D-1928, procedure C. Film obtained on a 50mm blow film line with barrier screw, 25:1 L/D, 1.0mm die gap, 50µm gauge, 2.3:1 BUR. Information provided by Dax Resinas Petroquimica Triunfo has been acquired by Braskem. |
FDA: 21 CFR 177.1520 (C) 2.1 |