System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
LTM 71L80-201 PVC
Categories:
Polymer
;
Thermoplastic
;
Vinyl (PVC)
Material Notes:
Thermoplastic elastomer flame retardant PVC series, Wire and cable grade, used in auto parts, electronic appliances, wire and cable, etc.
Information provided by Suzhou Long-term Materials Science Co., Ltd.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
<=
1.40
g/cc
<=
0.0506
lb/in³
ASTM D792
Deformation
8.0 %
@Temperature 150 °C,
Time 14400 sec
8.0 %
@Temperature 302 °F,
Time 4.00 hour
110?,3.5N; GB/T 2951.31
Mechanical Properties
Metric
English
Comments
Hardness, Shore A
85
@Time 15.0 sec
85
@Time 0.00417 hour
ASTM D2240
Tensile Strength
>=
20.0
MPa
>=
2900
psi
250mm/min; CQC1103-1105
Elongation at Break
>= 350 %
>= 350 %
250mm/min; CQC1103-1105
Tear Strength
>=
23.0
kN/m
>=
131
pli
250mm/min; CQC1103-1105
Thermal Properties
Metric
English
Comments
Brittleness Temperature
-50.0
°C
-58.0
°F
GB/T 5470-2008
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
PLTM022 / 296074
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.