MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Mockernut True Hickory Wood
Categories: Wood and Natural Products; Wood; Hardwood

Key Words: Carya Tomentosa; Lumber, Timber
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.640 g/ccGreen, based on volume
 0.720 g/cc12% moisture content, based on volume
 
Mechanical PropertiesOriginal ValueComments
Modulus of Elasticity 1570 ksiGreen
 2220 ksi12% moisture content
Modulus of Rupture 11.1 ksiGreen
 19.2 ksi12% moisture content
Compressive Strength 810 psiGreen, perpendicular to grain
 1730 psi12% moisture content, perpendicular to grain
 4480 psiGreen, parallel to grain
 8940 psi12% moisture content, parallel to grain
Shear Strength 1280 psiGreen, parallel to grain
 1740 psi12% moisture content, parallel to grain
Impact 77Impact bending in inches, 12% moisture content
 88Impact bending in inches, green
Work to Maximum Load 22.6 in-lb/in³12% moisture content
 26.1 in-lb/in³Green
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 1.20 BTU-in/hr-ft²-°FOven Dry, US origin
 1.40 BTU-in/hr-ft²-°F12% Moisture Content, US origin
Shrinkage 7.7 %Radial, from green to oven dry, US origin
 11 %Tangential, from green to oven dry, US origin
 17.8 %Volumetric, from green to oven dry, US origin

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Asian Mengkulang Wood
Honeylocust Wood
Japanese Oak Wood
Kauvula Wood
Laurel Red Oak Wood

PTSU023 / 71465

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.