MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

NIZHNEKAMSKNEFTEKHIM PP 4316M (EP1X35AF) Propylene and Ethylene Copolymer
Categories: Polymer; Thermoplastic; Polyethylene (PE); Polypropylene (PP)

Material Notes: Product obtained by copolymerization of propylene with ethylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation resistance when PP is produced, processed and PP-made articles are exploited, improved properties contributing to slipping and preventing from film layers sticking, and improved antistatic properties.

Information provided by manufacturer

Key Words: PP
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Melt Flow 7.0 - 10 g/10 min
@Load 2.16 kg,
Temperature 230 °C
7.0 - 10 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238/L
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield >= 29.0 MPa>= 4210 psiASTM D638
Elongation at Yield >= 10 %>= 10 %ASTM D638
Flexural Modulus >= 1.05 GPa>= 152 ksiASTM D790
Izod Impact, Notched >= 0.350 J/cm
@Temperature 23.0 °C
>= 0.656 ft-lb/in
@Temperature 73.4 °F
ASTM D256
 
Descriptive Properties
Gel Content (pcs./m²)0>= 2.5mm
 0(1.5-2.5)mm
 3(0.7-1.5)mm
 300>=0.2mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Braskem H 504 XP Bioriented Film Polypropylene
Hyosung Topilene F600 PP
Braskem H 401 Cast Film Extrusion Polypropylene
LyondellBasell Moplen HP528N Polypropylene
Buckeye Polymers BP RPPC 1813 C BLK Polypropylene, Calcium Filled

PNKNH036 / 109303

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.