Mondur MRS 2 is a low functionality polymeric diphenylmethane diisocyanate (pMDI) with a moderately high 2,4 ’-MDI isomer content. Properties / Applications: Mondur MRS 2 can be used in polyether and polyester molded flexible foams. It can also be used in the formulation of polyurethane binders, elastomers and adhesives. As with any product, use of Mondur MRS 2 in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability. Information provided by Covestro |