MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

NOVA Chemicals Sclair® 11H1 LLDPE Film Resin  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade

Material Notes: Low gel, Excellent heat sealability, Easy processability, High toughness and strength

Applications: Heavy duty sack, High strength packaging

Additives: Process stabilizer, Polymer process aid, Antiblock

Canada: The Health Protection Branch has indicated no objection to the sue in Canada of this resin for a variety of food packaging applications. Information on the packaging of specific foodstuffs should obtained from NOVA Chemicals or from the Health Protection Branch, Food Packaging Materials and Incidental Additives Section, Ottawa, Canada.
United States: This resin complies with the specification contained in the U.S. Food and Drug Administration (FDA) regulation 21 CFR 177.1520 for olefin polymer, para. (c) 3.2a, and may thus be used in the United States as an article or component of an article intended for use in contact with food.

Film properties are typical of blown film extruded at a blowup ratio of 2.5:1, but are dependent upon operating conditions.

Information provided by NOVA Chemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.920 g/cc0.0332 lb/in³ASTM D792
Thickness 25.0 - 75.0 microns0.984 - 2.95 mil
Melt Flow 0.80 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.80 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 9.50 MPa1380 psiASTM D882
Film Tensile Strength at Yield, TD 10.0 MPa1450 psiASTM D882
Film Elongation at Break, MD 640 %640 %ASTM D882
Film Elongation at Break, TD 770 %770 %ASTM D882
Secant Modulus, MD 0.190 GPa27.6 ksiat 1%; ASTM D882
Secant Modulus, TD 0.200 GPa29.0 ksiat 1%; ASTM D882
Impact 4848J/mm; NOVA Chemicals Puncture test
Coefficient of Friction 0.600.60ASTM D1894
Elmendorf Tear Strength, MD 20.0 g/micron508 g/milASTM D1922
Elmendorf Tear Strength, TD 24.0 g/micron610 g/milASTM D1922
Dart Drop 7.00 g/micron178 g/milF50, ASTM D1709/A
Film Tensile Strength at Break, MD 41.3 MPa5990 psiASTM D882
Film Tensile Strength at Break, TD 40.7 MPa5900 psiASTM D882
 
Optical PropertiesMetricEnglishComments
Haze 12 %
@Thickness 0.0254 mm
12 %
@Thickness 0.00100 in
ASTM D1003
Gloss 50 %50 %at 45°; 1 mil; ASTM D2457
 
Processing PropertiesMetricEnglishComments
Melt Temperature 220 - 230 °C428 - 446 °F
Die Opening 0.0900 - 0.220 cm0.0354 - 0.0866 in
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.
 
Descriptive Properties
Blow Up Ratio2:1 to 3:1

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNOVA098 / 54999

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.