MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 60 PHR N220 (ISAF) Filler
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Elastomer, Unreinforced; Rubber or Thermoset Elastomer (TSE)

Material Notes: MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outstanding hydrolytic stability and improved processing. MILLATHANE E34 can be compounded and processed by the use of conventional rubber manufacturing equipment — mixed on two roll mills or an internal mixer. Compounds can be — calendered; extruded; injection, transfer, or compression molded — to produce finished polyurethane parts. It can be vulcanized by organic peroxides or sulfur with thiazole accelerators..

All information provided by TSE Industries

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A >= 80>= 80
Tensile Strength 24.90 MPa3611 psi
Elongation at Break 442 %442 %
100% Modulus 7.598 MPa
@Strain 100 %
1102 psi
@Strain 100 %
200% Modulus 15.30 MPa
@Strain 200 %
2219 psi
@Strain 200 %
300% Modulus 20.50 MPa
@Strain 300 %
2973 psi
@Strain 300 %
Tear Strength 36.0 kN/m205 pliDie C
 
Processing PropertiesMetricEnglishComments
Cure Time 10.0 min
@Temperature 155 °C
0.167 hour
@Temperature 311 °F
Press cured
 
Descriptive Properties
DIN Abrasion (mm³)43.2
Formulation as Tested0.5Zinc Stearate
 0.5Struktol WB 222
 0.5Poly AC 617A
 1Thanecure® ZM
 1.5Sulfur
 10Cumar P10
 100Millathane E34
 2MBT
 4MBTS
 60Carbon Black N-220 (ISAF)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMILL411 / 87455

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.