MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
A. Schulman POLYBATCH™ White 8000 AP Concentrate Based In LDPE
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: Description

POLYBATCH® 8000 AP is an advanced performance white color concentrate containing 70% TiO2 based in LDPE. This product has been specifically engineered to provide improved resistance to phenolic yellowing/pinking while optimizing whiteness and thermal stability. This product also provides high opacity and excellent letdown mixing. POLYBATCH® 8000 AP is designed for use in extrusion film, sheet, injection, and blow molding applications.

Information provided by A. Schulman.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.04 g/ccASTM D792
Moisture Absorption <= 0.100 %ASTM D789
Melt Flow 7.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
Ash 70 %
 
Descriptive Properties
Pellet Count 28pellets/gram

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
A. Schulman POLYBATCH™ White 8350 AP Concentrate Based In LDPE
A. Schulman POLYBATCH™ White P8555 T2 Concentrate Based In Homopolymer Polypropylene
A. Schulman POLYBATCH™ White LL8844 GP
A. Schulman POLYBATCH™ ASC-331 Inorganic Antislip Masterbatch Based in Polyethylene
A. Schulman POLYBATCH™ White 8350 EC1 Concentrate Based In LDPE

PASHU491 / 25455

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.