MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Elastron® Elastron® G G500.A80.B.ABS SEBS
Categories: Polymer; Thermoplastic; Styrene-Butadiene

Material Notes: Product Description: A soft, black SEBS based thermoplastic elastomer (TPE) compound specially designed for excellent adhesion to ABS/PC/PMMA/SAN/ASA/PET and PET-G. The Bondable to: PMMA, ABS/PC, ASA, SAN, PET, PET-G
Availability: Africa & Middle East; Asia Pacific; Europe; North America
Features: Block Copolymer; Bondability; Good Adhesion; Soft
RoHS Compliance: RoHS Compliant
Appearance: Black
Forms: Pellets
Processing Method: Injection Molding

Information provided by Elastron

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.10 g/cc0.0397 lb/in³ASTM D792
Linear Mold Shrinkage, Flow 0.010 cm/cm0.010 in/inASTM D955
Linear Mold Shrinkage, Transverse 0.0065 cm/cm0.0065 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8080ASTM D2240
Tensile Strength at Break 18.0 MPa2610 psiASTM D412
Tensile Stress  3.30 MPa
@Strain 100 %
479 psi
@Strain 100 %
ASTM D412
 7.03 MPa
@Strain 300 %
1020 psi
@Strain 300 %
ASTM D412
Elongation at Break 700 %700 %ASTM D412
Tear Strength 55.0 kN/m314 pliASTM D624
Compression Set  25 %
@Temperature 22.8 °C,
Time 79200 sec
25 %
@Temperature 73.0 °F,
Time 22.0 hour
ASTM D395
 67 %
@Temperature 70.0 °C,
Time 79200 sec
67 %
@Temperature 158 °F,
Time 22.0 hour
ASTM D395
 86 %
@Temperature 100 °C,
Time 79200 sec
86 %
@Temperature 212 °F,
Time 22.0 hour
ASTM D395
 
Thermal PropertiesMetricEnglishComments
Flammability, UL94 HBHB
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 170 - 190 °C338 - 374 °F
Middle Barrel Temperature 180 - 200 °C356 - 392 °F
Front Barrel Temperature 190 - 200 °C374 - 392 °F
Nozzle Temperature 200 - 210 °C392 - 410 °F
Mold Temperature 40.0 - 60.0 °C104 - 140 °F
Drying Temperature 80.0 °C176 °F
Dry Time 3.00 hour3.00 hour
 
Descriptive Properties
Ozone ResistanceNo CracksStressed, ASTM D518
Suggested Max Regrind0.2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PELAST348 / 267930

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.