Platinum Ink C2040323D1 is a screen printable ink designed for printing working electrodes in electrochemical sensor applications. The ink is designed for firing polymer substrates, including high stability polymers such as Kapton. The ink has been made at a ready to use viscosity and should be thoroughly stirred before use avoiding introduction of air bubbles. It can be printed on automatic and semi automatic screen printers. Information provided by Gwent Electronic Materials Ltd. |