MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Beijing Chemical Industry KAIFA® M106N MPPO Resin
Categories: Polymer; Thermoplastic; Polyphenylene Ether/PPO

Material Notes: High Flame retardant, High thermal resistant

Information provided by Beijing Chemical Industry Research Institute (Group)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.07 g/ccASTM D792
Water Absorption 0.10 %24 hr; ASTM D570
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 60.0 MPaASTM D638
Elongation at Break 30 %ASTM D638
Flexural Strength 88.0 MPaASTM D790
Flexural Modulus 2.40 GPaASTM D790
Charpy Impact, Notched 1.50 J/cm²ISO179
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+16 ohm-cmASTM D257
Dielectric Constant 2.8
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 20.0 kV/mm
@Thickness 2.00 mm
ASTM D149
Dissipation Factor 0.0070
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 70.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 120 °CASTM D648
Flammability, UL94 V-0
@Thickness 3.20 mm
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 260 °C
Middle Barrel Temperature 280 °C
Front Barrel Temperature 280 °C
Nozzle Temperature 275 °C
Mold Temperature 80.0 °C
Injection Pressure 120 MPa
Cycle Time - Injection 35 sec
Screw Speed 70 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LG Chemical LUMILOY GN1006F Injection Molding FR mPPO
Beijing Chemical Industry KAIFA® M106 MPPO Resin
Beijing Chemical Industry KAIFA® M105N MPPO Resin
Beijing Chemical Industry KAIFA® M105 MPPO Resin
Beijing Chemical Industry KAIFA® M104N MPPO Resin

PKAIF53 / 48635

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.