MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Chemours Teflon™ 851G-221 High Film Build PTFE industrial coating
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes: Teflon™ PTFE (polytetrafluoroethylene) industrial coatings have: The highest operating temperature of any fluoropolymer (260 °C [500 °F]). The lowest coefficient of friction. Good abrasion and chemical resistance. PTFE industrial coatings are commonly used in mold release applications for products such as golf balls and rubber mats, but can be utilized in multiple applications and uses. These PTFE coatings for multi-coat systems are only available as a water-based liquid.

Information provided by Chemours.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Water Absorption <= 0.010 %
@Time 86400 sec
<= 0.010 %
@Time 24.0 hour
ASTM D570
Thickness 20.3 - 76.2 microns0.800 - 3.00 milFilm Build per coat
 <= 203 microns<= 8.00 milMax Total Film Build
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 260 °C500 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 399 °C750 °FCure Temperature
 
Compliance PropertiesMetricEnglishComments
FDA NoNoFood Contact per 21CFR.
 
Descriptive Properties
CarrierWater
Chemical/Solvent ResistanceExcellentASTM D543
ColorGray
Detergent Resistance (hours)24On grit blasted aluminum
 264
 624On aluminum
Salt Spray Resistance Coatings (hours)192ASTM B117. 5% NaCl at 35 °C (95 °F). On aluminum.
 744+ASTM B117. 5% NaCl at 35 °C (95 °F).
Weather Resistance (years unaffected)20Florida Exposure

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDU8725 / 268651

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.