MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Eastman Benzoflex™ 354 Plasticizer
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Product Description: Benzoflex™ 354 is a high solvating, non-phthalate plasticizer compatible with a wide range of synthetic resinous materials, and it imparts a softening and flexibilizing effect to these resins. Benzoflex™ 354 is suggested for use as a resin plasticizer/modifier in the formulation of specialty coatings and adhesives and PVC plastisols.

Application/Uses:

  • Automotive
  • Coatings
  • Decals/Graphics/Graphic Arts
  • Flexible PVC
  • PVC plastisols

Information provided by Eastman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.08 g/cc0.0390 lb/in³
Viscosity 634 cP634 cP
Vapor Pressure 0.00000122 bar0.000912 torr
 
Thermal PropertiesMetricEnglishComments
Melting Point -12.0 °C10.4 °FFreezing Point
Boiling Point >= 300 °C>= 572 °F
Flash Point 197 °C387 °FSetaflash Closed Cup
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.531.53
 
Descriptive Properties
Acidity<0.1%
ColorPt-Co

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEATM5076 / 222270

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.