MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Eastman TREVA™ OP6026NAT Natural Cellulosic Engineering Bioplastic
Categories: Polymer; Thermoplastic; Cellulosic; Polylactic Acid (PLA) Biopolymer

Material Notes: Eastman TREVA™ is a cellulose-based engineering bioplastic that offers both high performance and reduced environmental impact. TREVA is warm to touch, dimensionally stable and offers excellent flow and easy polish and paint for processing.

Applications

  • Eyewear
Key Attributes
  • Dimensional stability
  • Easy polish and paint
  • Excellent flow
  • Warm touch and feel

Information provided by Eastman.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.22 g/ccASTM D792
Water Absorption 2.30 %
@Time 86400 sec
immersion; ASTM D570
Linear Mold Shrinkage 0.00700 in/inASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 100ASTM D785
Tensile Strength at Break 48.0 MPaASTM D638
Tensile Strength, Yield 49.0 MPaASTM D638
Elongation at Break 18.0 %ASTM D638
Flexural Modulus 1940 MPaASTM D790
Izod Impact, Notched 100 J/m
@Temperature -40.0 °C
ASTM D256
 216 J/m
@Temperature 23.0 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 114 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 99.0 °CASTM D648
Vicat Softening Point 135 °CConditioned 4 hours at 70°C; ASTM D1525
 
Processing PropertiesOriginal ValueComments
Processing Temperature 235 °CBarrel Set Temperature
Mold Temperature 85.0 °C
Injection Velocity 30.0 mm/sec
Drying Temperature 75.0 °Cin a Desiccant Dryer
Dry Time 4.00 hourin a Desiccant Dryer
 
Descriptive Properties
Maximum Barrel Residence Time4 minutes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEATM4162 / 323785

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.