System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Taro Plast Haiplen H50 TC8 PP, 40% Talc Filled
Categories:
Polymer
;
Thermoplastic
;
Polypropylene (PP)
;
Polypropylene with 40% Talc Filler
Material Notes:
Polypropylene homopolymer 40% talcum filled for aesthetic applications. Available: all colors, UV stabilized (L), heat stabilized (H), laser printable (LP), detergent stabilized (D).
Information provided by Taro Plast S.p.a.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.25
g/cc
0.0452
lb/in³
ISO 1183
Filler Content
40 %
40 %
ISO 3451
Water Absorption
0.050 %
@Time 86400 sec
0.050 %
@Time 24.0 hour
ISO 62
Linear Mold Shrinkage, Flow
0.0090
cm/cm
0.0090
in/in
ISO 2577
Linear Mold Shrinkage, Transverse
0.0090
cm/cm
0.0090
in/in
ISO 2577
Melt Flow
10
g/10 min
@Load 2.16 kg,
Temperature 230 °C
10
g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties
Metric
English
Comments
Tensile Strength, Yield
33.0
MPa
4790
psi
ISO 527
Elongation at Break
25 %
25 %
ISO 527
Tensile Modulus
3.90
GPa
566
ksi
ISO 527
Flexural Modulus
3.70
GPa
537
ksi
ISO 178
Izod Impact, Notched
0.180
J/cm
@Temperature -20.0 °C
0.337
ft-lb/in
@Temperature -4.00 °F
127x12.7x3.2; ASTM D256
0.420
J/cm
@Temperature 23.0 °C
0.787
ft-lb/in
@Temperature 73.4 °F
127x12.7x3.2; ASTM D256
Charpy Impact, Notched
0.400
J/cm²
1.90
ft-lb/in²
80x10x4; ISO 179/1eA
Electrical Properties
Metric
English
Comments
Comparative Tracking Index
>=
600
V
>=
600
V
Method A; IEC 60112
Thermal Properties
Metric
English
Comments
CTE, linear
60.0
µm/m-°C
33.3
µin/in-°F
ISO 11359
Hot Ball Pressure Test
125
°C
257
°F
IEC 60695-10-2
Deflection Temperature at 1.8 MPa (264 psi)
82.0
°C
180
°F
ISO 75/A
Vicat Softening Point
94.0
°C
@Load 5.00 kg
201
°F
@Load 11.0 lb
ISO 306
155
°C
@Load 1.00 kg
311
°F
@Load 2.20 lb
ISO 306
Flammability, UL94
HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
127x2.17xThickness
Oxygen Index
21 %
21 %
6.3x12.7x3.2; ASTM D2863
Glow Wire Ignition Temperature
550
°C
@Thickness 1.60 mm
1020
°F
@Thickness 0.0630 in
60x60xThickness; IEC 60695-2-13
Glow Wire Flammability Index
650
°C
@Thickness 1.60 mm
1200
°F
@Thickness 0.0630 in
60x60xThickness; IEC 60695-2-12
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
PTARO123 / 283231
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.