Hostacom ERC 450N R is a 10% talc filled PP copolymer compound, with superior flowability, low density, excellent scratch resistance, offering low odor and low emissions performances. Advanced technologies allowed for a significant reduction of mineral filler which contributed to the reduction of final part weight. This polypropylene compound is produced locally in Russia. Availability: Europe Application: Automotive Parts; Instrument Panels; Interior Automotive Applications Market: Automotive Processing Method: Injection Molding Attribute: Excellent Processability; Excellent Stiffness; Good Abrasion Resistance; Good Color Stability; Good Impact Resistance; Good Surface Finish; High Flow; Low Density; Low to No Odor; Low VOC Emission; Scratch Resistant; UV Resistant Information provided by LyondellBasell. |