MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Chesterton 814 Sump Cleaner & Conditioner  (discontinued **)
Categories: Fluid

Material Notes: Description: Chesterton® 814 Slum Cleaner & Conditioner is a highly concentrated non-foaming alkaline cleaner specifically designed to clean and condition metal working fluid sumps and circulation pipework. Regular use of 814 at sump change outs improves rancidity control by removing dirt, grit, metal fines, insoluble soaps and emulsion oils that create the breeding ground for bacteria and fungus. 814 is a versatile cleaner that can be used in all parts of the metal processing industry. 814 is designed for the toughest cleaning jobs such as decontaminating and removing residues from rancid central sump systems in hard water areas.

Features:

  • Concentrated
  • Virtually Non-Foaming
  • Corrosion Inhibited
  • No Residue
  • Excellent Demulsibility
  • Wide Dilution Range
Applications: Recommended for the cleaning and conditioning of individual machines, central circulation reservoirs, mix tanks, pipework, tooling, finished parts, floors and all surfaces contaminated with machining or cutting fluids or oils.

Information provided by Chesterton

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.05 g/cc1.05 g/cc
pH 10.210.21% dilution
 11.711.75% Concentration
 12.212.210% Concentration
 12.512.550% Concentration
 13.413.4100% Concentration
 
Descriptive Properties
AppearanceYellow liquid, slightly hazy

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPTCHS055 / 138167

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.