MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Amity Thermosets AMP 481 Phenolic Molding Organic and inorganic Filler, Compression Molded
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Phenolic

Material Notes:

Characteristics:

  • Good tracking resistance
  • Good dielectric strength
  • Good electrical insulation
  • Applications:

  • Switchgear components which ought to have high tracking resistance
  • Circuit protecting switches
  • Micro switches etc.
  • Information provided by Amity Thermosets Limited

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesOriginal ValueComments
    Density 1.40 - 1.45 g/ccMolding; IS 867-1963
    Apparent Bulk Density 0.620 - 0.700 g/ccIS 867-1963
    Water Absorption <= 0.40 %IS 13411-1993
    Linear Mold Shrinkage 0.0040 - 0.0075 cm/cmbar; IS 13411-1992
     0.0060 - 0.0075 cm/cmdisk; IS 13411-1992
     
    Mechanical PropertiesOriginal ValueComments
    Tensile Strength at Break 56.0 - 70.0 MPa5 mm/min.; IS 867-1963
    Shear Strength 75.0 - 90.0 MPa2mm/min.; IS 867-1963
    Izod Impact, Notched 22.0 - 35.0 J/mIS 13411-1992
     
    Electrical PropertiesOriginal ValueComments
    Volume Resistivity 1.00e+11 - 3.16e+11 ohm-cmIS 3396-1979
    Surface Resistance 1.00e+10 - 1.00e+11 ohmIS 3396-1979
    Dielectric Strength >= 7.00 kV/mm
    @Temperature 90.0 °C
    IS 2584-1963
    Comparative Tracking Index >= 300 V2824-1975
     
    Processing PropertiesOriginal ValueComments
    Mold Temperature 160 - 180 °C
    Injection Pressure 15.68 - 34.3 MPaMold Pressure
    Cure Time 25.0 - 35.0 secper mm
    Shelf Life 4.00 Month10-25°C

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

    Users viewing this material also viewed the following:
    Reltek BONDiT™ B-481 Adhesive, Sealant & Coating System
    Tra-Con Tra-Bond Ablebond 481-20 B-Stageable Epoxy Adhesive
    Amity Thermosets ATM 122 Phenolic Molding Organic Filler, Compression Molded
    Amity Thermosets ATI 172 Phenolic Molding Organic and inorganic Filler, Injection Molded
    Amity Thermosets ATI 102 Phenolic Molding Organic Filler, Injection Molded

    PAMITY36 / 24064

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.