MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Master Bond Supreme 11AO Electrically Isolating Adhesive and Sealant
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Description: Master Bond Polymer System SURPEME 11AO is a two component epoxy resin system for high performance bonding and sealing formulated to cure at room temperature or more rapidly at elevated temperatures with a convenient one-to-one (1:1) mix ratio by weight or volume. Its most outstanding features include high thermal conductivity, excellent electrical insulation properties, temperature resistance up to 250°F as well as superior bond strength. SURPEME 11AO is a paste that can be applied without sagging or dripping even on vertical surfaces. As a toughened system, it is well suited to applications involving thermal cycling. Its chemical resistance profile includes water, oils and most organic solvents. It has excellent adhesion to most metals, ceramics, glass and vulcanized rubbers as well as many plastics. SURPEME 11AO is also unique in that the bond strength is high in both shear and peel modes. Both part A and B are colored off-white. Master Bond SURPEME 11AO is widely used in the electronic,. electrical, computer, metalworking, appliance, automotive and chemical industries where high bond strength and superior heat transfer properties are required.

Product Advantages:

  • Easy application; adhesive spreads evenly and smoothly.
  • Versatile cure schedules; ambient temperature cures or faster elevated temperature cures as required.
  • High bond strength to a wide variety of substrates; excellent adhesive properties.
  • High thermal conductivity with exceptional electrical insulation properties.
  • Toughened system; well suited for bonding dissimilar substrates.
  • Good physical strength characteristics; especially high shear & peel strengths.
  • Thick paste; non-drip type system.
  • Outstanding resistance to a wide range of chemicals.
  • Thermally stable up to 250°F with good thermal cycling properties.

Information provided by MasterBond®

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Water Absorption <= 1.0 %24 hr immersion
 
Mechanical PropertiesOriginal ValueComments
Shear Strength 1540 psiBond, Al to Al, after 30 days water immersion
 1600 psiBond, Al to Al, RT cure
Peel Strength >= 15.0 pliT-peel, Al to Al
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength >= 400 V/mil
@Thickness 3.17 mm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 30.0 - 35.0 µm/m-°C
Thermal Conductivity 10.0 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 250 °F
Minimum Service Temperature, Air -100 °F
Glass Transition Temp, Tg 75.0 - 80.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 1.00 - 2.00 hour
@Temperature 93.3 °C
 24.0 - 36.0 hour
@Temperature 23.9 °C
Pot Life 25 - 30 min200 gram mass
 30 - 40 min100 gram mass
Shelf Life 6.00 Month
@Temperature 23.9 °C
unopened containers
 
Descriptive Properties
Mixing Ratio (A to B)1/1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMASTB350 / 149597

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.