MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Copper Thermocouple Wire Type T - Standard
Categories: Metal; Nonferrous Metal; Copper Alloy; Pure Element

Material Notes: All values may vary dependent on specific design and usage

Capabilities:

  • Wire
  • Ribbon
  • Square
  • Insulated
  • Plated

Information provided by California Fine Wire.

Key Words: ASTM E230
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.323 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 30000 psiAnnealed
 45000 psiStress relieved
 55000 psiHard
Tensile Strength, Yield 10000 psiAnnealed
 35000 psiStress relieved
 40000 psiHard
Modulus of Elasticity 17000 ksi
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 10.3 ohm-cir-mil/ft3% tolerance on sizes below 0.02, 5% tolerance on sizes above 0.02
 
Thermal PropertiesOriginal ValueComments
CTE, linear 17.0 µm/m-°C
@Temperature 20.0 °C
Specific Heat Capacity 0.385 J/g-°C
@Temperature 20.0 °C
Thermal Conductivity 391 W/m-K
Melting Point 1981 °F
Maximum Service Temperature, Air 300 °COperating Temperature
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 99.99 %
 
Descriptive Properties
MagneticNone
Temperature Coefficient of Resistance0.00394 ohms/ohm-°C0-100°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Copper, UNS C12100
Copper, UNS C12000
Overview of materials for Copper Alloy
EMS-Grivory Grilamid® L 16 W 20 black 9995 PA12

MTC03 / 14221

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.